Mesh welding machine welder strength is uneven

Views:0     Author:Site Editor     Publish Time: 2018-12-18      Origin:Site Inquire

Fault phenomenon 4:The welding spot strength of the mesh welding machine is not uniform or there are individual welding points not welded

Causes and elimination of faults:The key to such problems is caused by uneven upper and lower welding electrodes or uneven surface contact and uneven welding electrode pressure.In general,it is because the contact faces of the upper and lower welding electrodes are used for a long time.If the flat surface is uneven (with grooves) or the splash particles such as oxide scale and brushed powder affect the welding of the workpiece,the grinding electrode can be solved.

In the event of such a failure,it may be caused by severe oxidation of the surface of the welded steel material,rust or too much deposit of the drawn powder.At this time,it is necessary to treat the surface of the steel to be welded before performing the welding operation.


Product Inquiry
Hebei Jiaoyang Wire Mesh Machine Co.,ltd.
Add: no.28 weier road,eastern industrial zone,anpingcounty,hebei 
Email:
weldingmachine@jiaoyangen.net
Tel: +86-13932830858
Copyright
 2017 Hebei Jiaoyang Wire Mesh Machine Co., Ltd.  All rights reserved.
Support by 
Rongchuangmedia  
sitemap.xml

Quick Navigation

Product Category